High chromium cast irons (HCCI’s) exhibit very good mechanical properties and offer benefits for a range of manufacturing applications.
One of the main flexibilities exhibited is the possibility of HCCI’s to have different matrix structures in different treatment states whether it be austenite in casting state, pearlite in annealing state, martensite in quenching state, and tempered martensite in tempering state.