Titanium powder metallurgy can produce high performance and low cost titanium parts. Compared with those by conventional processes, high performance P/M titanium parts have many advantages: excellent mechanical properties, near-net-shape and low cost, being easy to fabricate complex shape parts, full dense material, no inner defect, fine and uniform microstructure, no texture, no segregation, low internal stress, excellent stability of dimension and being easy to fabricate titanium based composite parts.