Copper and copper alloys are specific in their corrosion behavior in that the initial corrosion rate of this group of materials is relatively high until protective layers form according to the alloy and the composition of the electrolytic solution.
One prime example of a material group which has found widespread use within the marine environment due to its excellent corrosion resistance are the copper-nickel alloys.
Category Archives: Corrosion
Corrosion Behaviour of Copper Alloys: Part One
Copper demonstrates excellent corrosion resistance in marine environments as well as showing strong abilities to withstand several other key localized corrosion forms which could potentially lead to failure.
Commonly weathered copper will go through a range of visual appearance transformations including the development of a brown patina within a few days of exposure and this will develop into the recognized green color over a period of 7-9 years.
Corrosion Protection of Steel: Part Two
Metallic coatings provide a layer that changes the surface properties of the work piece to those of the metal being applied. The work piece becomes a composite material exhibiting properties generally not achievable by either material if used alone.
Metallic coatings are deposited by electroplating, electroless plating, spraying, hot dipping, chemical vapor deposition and ion vapor deposition.
Corrosion protection of Steel
Corrosion of steel is an electrochemical reaction that requires the presence of water (H2O), oxygen (O2) and ions such as chloride ions (Cl–), all of which exist in the atmosphere. Electrophoretic deposition is a process in which electrically charged particles are deposited out of a water suspension to coat a conductive part. The process is more commonly known as electrocoating or E-coating.
Titanium Corrosion Properties: Part One
Titanium is well known for its extremely tough characteristics in severe environments with specific applications in the chemical process industry, energy, desalination, military and many more.
The most important properties of titanium in relation to corrosion resistance are its immunity to both pitting and stress corrosion.
Hydrogen Sulfide Corrosion
Hydrogen sulfide corrosion and its prevention is an important topic in a range of industrial processes and environments including oil and gas and its related activities.
Mild steel is a popular structural steel in this industry but is susceptible to surface scale formation and associated corrosive action, the prevention of which requires some special methods.
Corrosion of Aluminum and Its Alloys: Forms of Corrosion
Corrosion is the chemical reaction of a metal, in this case aluminum, with its environment, which leads to the deterioration of the properties of metals, aluminum in this case. Aluminum is a very reactive metal, but it is also a passive metal. This contradictory nature is explainable because nascent aluminum reacts with oxygen or water and forms a coherent surface oxide which impedes further reaction of aluminum with the environment.