Continuous Electroplating Process for Steel Sheet Products

The steel sheet electroplating process utilizes the same basic principle as that for conventional decorative finish electroplating. However, the steel sheet process differs in that the electroplated coating is applied by passing the strip at high speeds through a series of plating cells, building the coating thickness by a small amount each time the strip passes through an individual cell.
Continue reading