Wrought Aluminum Alloys for General and Special Applications: Part One

The main groups of aluminum alloys which are the most often used in practice besides technically pure aluminum are AlMn, AlMg, AlMgMn, AlMgSi, AlZnMg, and AlZnMgCu alloys. These are wrought alloys which are shaped into products by rolling, extrusion, and forging. Each of the mentioned groups consists of numerous subgroups, depending on amounts of main and additional alloying elements, and they have tensile strength values varying in a wide range from 70 to 600 MPa.

Continue reading