Heat treatment can be performed on ductile iron to increase strength, wear resistance, ductility, toughness, and/or improve machinability by controlling the matrix microstructure. In ferrous alloys, an intercritical heat treatment starts with partial austenitization in the intercritical region where ferrite and austenite are present. The amount of austenite depends on the chemistry of the alloy and the temperature. Continue reading